Deltawrap CFW

Carbon Fibre Fabric Strengthening System

DESCRIPTION

Deltawrap CFW is a carbon fibre fabric material for structural strengthening system. Applied with a two components primer Deltawrap primer, and finished by Deltawrap Encapsulation Resin Coating for an integrity result.

USES

Increasing the strength of reinforced concrete to anticipate the change of flexural and shear load due to : increase of loading capacity, changes of building utilization, repairing of defects, etc. It can be applied on beams, columns, walls, floor slabs, etc.

ADVANTAGES

  • Very high strength
  • Improve flexural and shear capacity
  • Flexible to any geometry surface (square, round, curve, etc)
  • Anti corrosion and easy to apply

INSTRUCTION FOR USE

Deltawrap CFW is cut able by a special scissors or knife, but can not be folded.

 

APPLICATION

Base Concrete Preliminary Preparation

The concrete should be well setting (28 days as a minimum age)

Prepare the substrate by sandblasting or grinding. Then cleaning it from dust, loose particles, grease, and oil. It should be dry and leveled by using epoxy putty. The adhesive tensile strength of the substrate to be reinforced must be at least 1.0 N/mm2

Mixing for Deltawrap Primer

Separately, mix each component in their container. Then add component B to component A using an electric mixer for approx. 3 minutes, until all the coloured streaks have disappeared. Then, stir again for approx 1 minute at low speed in a clean container to keep air entertainment at a minimum.

When the two components are mixed, then the pot life is starting. The lower ambient temperature, the longer pot life should be. And the higher quantity of material mixed, the shorter of pot life is.

Application of Primer Coating

Apply the mixed resin Deltawrap Primer to the prepared substrate using a trowel or brush.

Adhesion of Deltawrap CFW

Place the Deltawrap CFW onto the coating in a required direction.

 

Resin Impregnation

Due to an integrity result, after the Deltawrap CFW installed, finish it by coating Deltawrap Encapsulation Resin in 4 – 6 hours later.

TECHNICAL DATA

  1. Deltawrap CFW
Type Carbon Fibre Fabric
Fibre Areal Weight 300 g/m2
Fabric Design Thickness 0.166 mm
Fibre Tensile Strength 4,900 MPa
Fibre Tensile E-Modulus 230 GPa
Elongation at Break 2.1 %
Fabric Dimension W : 50 cm L : 100 m
Shelf life Unlimited
Package 1 roll in plain card board box
  1. Deltawrap Primer
Type Epoxy Resin
Adhesive Strength >1.5 Mpa (Design) ; 2.4 Mpa (Actual)
Shear Strength >30 MPa
Compressive Strength >60 MPa
Flexural Strength >40 MPa
Flexural E Modulus >3500 MPa
Application Temperature 5 - 350 C
Viscosity (cps @ 250 C) <2000
Shelf life 1 year
Coverage 0.3 kg /m2
Package Hardener (5 kg), Base Resin (10 kg), Mixing Ratio 1 : 2
  1. Deltawrap Encapsulation Resin
Type Fabric Impregnation Resin
Adhesive Strength >1.5 Mpa (Design) ; 2.4 Mpa (Actual)
Shear Strength >30 MPa
Compressive Strength >60 MPa
Flexural Strength >40 MPa
Flexural E Modulus >3500 MPa
Application Temperature 5 - 350 C
Viscosity (cps @ 250 C) <2000
Shelf Life 1 year
Coverage 0.825 kg /m2
Package Hardener (5 kg), Base Resin (10 kg), Mixing Ratio 1 : 2

 

HEALTH AND SAFETY

Deltawrap CFW, Deltawrap Primer and Deltawrap Encapsulation Resin may caused harm in some skin contact,avoid contact with skins, eyes and inhalation of vapor. Protective gloves and eyes protection are highly recommended during work of application.

Our Location

PT. Deltacretindo Wira Mandiri
  JL. Pintu Air IV No. 41A
  Jakarta, Indonesia 10710
  +62-21-344 2919
  +62-21-3511 428
  +62-811-9119-611
   :  deltacrete@gmail.com

haki cm

Print
© 2017 Deltacretindo. All Rights Reserved. Powered By GM-Portalindo